Technology and quality

Tested at the bench, not in the brochure

A COB strip fails in three places: the phosphor line, the solder joint, and the reel. Each one has a test before the batch leaves the building.

COB strip on a reel lit as one continuous line, no visible LED dots

Test 01

Aging test

Every batch is run lit before it is packed.

Reels and boards are powered for an aging run before packing so a phosphor or solder fault shows up at the bench rather than on site.

Close-up of a COB strip: chips on board under one continuous phosphor line

Test 02

Thermal shock

Boards cycle between hot and cold to test the solder joint.

Samples move between high and low temperature to check that the solder joint and the PCB coating survive the swing a fixture sees in service.

Finished COB strip reel being wound on the line

Test 03

Rewind and tension

Reels are pulled to catch a weak solder point or a lifted chip.

Finished reels are rewound under tension, which surfaces a joint that only looks sound until it is flexed on the reel.

How the spec fields are read

The same six fields appear on every product page. These are the definitions we quote against.

LEDs / m
Density of the COB line. Read it with watts per metre — the two decide the light level together.
Cut interval
The shortest length the strip can be cut and still work. Set your run length against this number.
PCB width
3 mm to 30 mm depending on density. The extrusion has to take the width plus clearance.
Feed length
How far one feed can carry the run. 48V boards hold 20 m from one end; 12V reels stay at 5 m.
CRI
Ra > 90 across the standard white range, Ra > 80 on the mains voltage series. Colour and RGB strips are not rated for CRI.
CCT
2700K, 3000K, 4000K and 6000K as standard, with 3500K on selected models and 2700K–6500K on tunable white.

From incoming board to a labelled reel

01

Incoming board and phosphor

PCB, chips and phosphor are checked against the ordered bin and width before a reel is built.

02

Assembly and sealing

Density, cut interval and coating follow the model sheet for that reel or board.

03

Bench testing

Aging, thermal shock and rewind checks are run on the batch before it is released.

04

Packing and documentation

Reels are labelled with model, voltage, CCT and cut interval so the site team can match them.

Need a test report or a sample for a specific model? Ask for it by model number.